Armstrong X-81-A/F Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Armstrong Epoxy Adhesives; Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Armstrong X-81-A/F Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ellsworth Adhesives.
Physical Properties Metric English Comments
Viscosity 5000 cP
5000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Tensile Strength, Ultimate 44.5 MPa
6450 psi
after optimum cure
Elongation at Break 2.3 %
2.3 %
Adhesive Bond Strength 30.7 MPa
4450 psi
Steel-Steel; after optimum cure
10.3 MPa

@Temperature 82.2 °C
1500 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
14.1 MPa

@Temperature -54.4 °C
2050 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 104 °C
219 °F
Processing Properties Metric English Comments
Processing Temperature 22.2 °C
72.0 °F
73.9 °C
165 °F
Optimum cure is 2 hr. @ 165°F
Pot Life <= 6.00 min

@Temperature 25.0 °C
<= 6.00 min

@Temperature 77.0 °F
100 g
Descriptive Properties Value Comments
Color White
Mix Ratio 100/20/10
By Weight