Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 11.3 MPa | 1640 psi | 14 Day Cure; ASTM C882 |
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,.. |
|||
Adhesive Bond Strength | 11.3 MPa | 1640 psi | Lap shear, alum to alum, 8 min @ 150°C |