Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | >= 2.00 MPa | >= 290 psi | Butyl rubber, Substrate Failure, Shear; ISO 4587 |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Adhesive Bond Strength | >= 2.00 MPa | >= 290 psi | Butyl Rubber, Substrate Failure, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 2.00 MPa | 290 psi | Gum rubber, Shear; ISO 4587 |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Adhesive Bond Strength | 2.00 MPa | 290 psi | Butyl-Butyl; Substrate Failure; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Adhesive Bond Strength | >= 2.00 MPa | >= 290 psi | Butyl Rubber, Substrate Failure, Shear; ISO 4587 |
Permabond 910FS Cyanoacrylate, Methyl grade PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts.. |