Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 20.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 20.3 MPa
2950 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound
TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required..
Adhesive Bond Strength 20.3 MPa

@Temperature -54.4 °C
2950 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio
Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati..
Adhesive Bond Strength 20.3 MPa

@Temperature 25.0 °C
2950 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-3/E Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Adhesive Bond Strength 20.3 MPa
2950 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Tra-Con Tra-Bond 516H01 Low Viscosity Room Temperature Cure Adhesive
TRA-BOND 516H01 is a room temperature curing, low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors, including Pre-Mixed and Frozen applications. It has also been use..
Copyright © lookpolymers.com All Rights Reserved