Polymer Property : Adhesive Bond Strength = 3.00 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0207 MPa
3.00 psi
Arlon SQA-TMS-011
Arlon 51976XA015 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene