Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | >= 4.00 MPa | >= 580 psi | Nitrile rubber, Substrate Failure, Shear; ISO 4587 |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Adhesive Bond Strength | >= 4.00 MPa | >= 580 psi | Nitrile Rubber, Substrate Failure, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Acrylic, Shear; ISO 4587 |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Phenolic, Shear; ISO 4587 |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 4.00 - 6.00 MPa | 580 - 870 psi | FRP Glass/Epoxy, Shear; ASTM D1002 |
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 4.00 - 6.00 MPa | 580 - 870 psi | Carbon Fiber, Shear; ASTM D1002 |
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Steel to Ferrite using Initiator 41 after 3 minutes, Shear |
Permabond TA437 Toughened Acrylic Adhesive PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Steel to Ferrite after 3 minutes, Shear |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Ferrite/steel after 3 mins, Shear |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Ferrite/steel after 3 mins, Shear |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Steel to Ferrite, after 3 minutes, Shear |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Adhesive Bond Strength | >= 4.00 MPa | >= 580 psi | Plexiglass, Shear |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Adhesive Bond Strength | >= 4.00 MPa | >= 580 psi | PET, Shear |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | ABS, Shear; ISO 4587 |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Valox, Shear; ISO 4587 |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Adhesive Bond Strength | >= 4.00 MPa | >= 580 psi | Nitrile Rubber, Substrate Failure, Shear; ISO 4587 |
Permabond 910FS Cyanoacrylate, Methyl grade PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Phenolic, Shear; ISO 4587 |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Phenolic, Shear; ISO 4587 |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 4.00 MPa | 580 psi | Phenolic, Shear; ISO 4587 |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |