Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 3.50 - 48.3 MPa @Temperature -55.0 - 260 °C |
508 - 7010 psi @Temperature -67.0 - 500 °F |
Average value: 17.0 MPa Grade Count:77 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |