Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.50 - 48.3 MPa

@Temperature -55.0 - 260 °C
508 - 7010 psi

@Temperature -67.0 - 500 °F
Average value: 17.0 MPa Grade Count:77
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Adhesive Bond Strength 3.50 MPa
508 psi
Polystyrene, Shear; ISO 4587
Permabond 919 Cyanoacrylate, High temperature
Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I..