Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 56.9 MPa | 8250 psi | Steel-Steel; after optimum cure |
Armstrong A-4/E Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |