Polymer Property : 300% Modulus = 0.000280 GPa
Polymer Property :
300% Modulus =
0.000280 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
300% Modulus
0.000280
GPa
0.0406
ksi
UBE UBEPOL BR150B Synthetic Rubber (Compound)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.