Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00220 - 0.00650 GPa | 0.319 - 0.943 ksi | ASTM D 638 |
API Megol AM DP1741 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
300% Modulus | 0.00220 GPa | 0.319 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00220 GPa | 0.319 ksi | ISO/R527 |
Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |