Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00220 - 0.00650 GPa
0.319 - 0.943 ksi
ASTM D 638
API Megol AM DP1741 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..