Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00343 GPa | 0.498 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Mistron Vapor Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00343 GPa | 0.498 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Mistron Vapor Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00343 GPa | 0.497 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6070 BK Thermoplastic Elastomer DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in the injection molding process. DGR 6070NC has an excellent soft touch feel, will bond t.. |