Material Notes:
DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in the injection molding process. DGR 6070NC has an excellent soft touch feel, will bond to olefinics, is easy to color, and is available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal conditions does not require drying.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 0.985 g/cc
0.985 g/cc
ASTM D471
Viscosity 130000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
130000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
5 Sec; ASTM D2240
Tensile Strength at Break 8.34 MPa
1210 psi
ASTM D412
Elongation at Break 640 %
640 %
ASTM D412
100% Modulus 0.00262 GPa
0.380 ksi
ASTM D412
300% Modulus 0.00343 GPa
0.497 ksi
ASTM D412
Graves Tear Strength 28.6 kN/m

@Temperature 24.0 °C
163 pli

@Temperature 75.2 °F
Die C; ASTM D624
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F