Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.00380 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00380 GPa
0.551 ksi
ISO/R527
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based
Information provided by Polykemi AB
300% Modulus 0.00380 GPa
0.551 ksi
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 79 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
300% Modulus 0.00380 GPa
0.551 ksi
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
300% Modulus 0.00380 GPa
0.551 ksi
ISO 37
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane
AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh..
300% Modulus 0.00380 GPa

@Temperature 23.0 °C
0.551 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
300% Modulus 0.00380 GPa
0.551 ksi
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv..
300% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4520 Molded Golf Grip
FormulationNordel® IP 4520
300% Modulus 0.00380 - 0.00920 GPa
0.551 - 1.33 ksi
ASTM D 638
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..