Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesive for inks and lacquers, fabric coating and magnetic media binderAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Viscosity 92000 cP

@Temperature 204 °C
92000 cP

@Temperature 399 °F
Melt; ASTM D1084-88
Brookfield Viscosity 250 cP
250 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF
1600 cP
1600 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D412/D638
Elongation at Break 630 %
630 %
ASTM D412/D638
100% Modulus 0.00230 GPa
0.334 ksi
300% Modulus 0.00380 GPa
0.551 ksi
Peel Strength 0.120 kN/m
0.685 pli
to PET; TP-141
1.80 kN/m
10.3 pli
Aluminum Foil; ASTM D-1876-72
3.40 kN/m
19.4 pli
Mylar Film; ASTM D-1876-72
Thermal Properties Metric English Comments
Softening Point 85.0 °C
185 °F
Kofler; ASTM D1525
Glass Transition Temp, Tg -31.0 °C
-23.8 °F
DSC
Ring & Ball Softening Point 179 °C
354 °F
ASTM E28-94
Descriptive Properties Value Comments
Gradient Bar Tack Temperature 91°C
Open Time >300 sec
ASTM D-4497-94