Polymer Property : 300% Modulus = 0.00440 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00440 GPa
0.638 ksi
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
300% Modulus 0.00440 GPa
0.638 ksi
ASTM D 638
API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..