Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00440 GPa | 0.638 ksi | |
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
300% Modulus | 0.00440 GPa | 0.638 ksi | ASTM D 638 |
API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |