Polymer Property : 300% Modulus = 0.0250 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0250 GPa
3.63 ksi
ISO 37
Huntsman AVALON® 95 AHT DP Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.0250 GPa
3.63 ksi
DIN 53504
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
300% Modulus 0.0250 GPa
3.63 ksi
DIN 53504
Huntsman IROGRAN® A 98 P 4535 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer
PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou..
300% Modulus 0.0250 GPa
3.63 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane
Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil..
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
300% Modulus 0.0250 GPa
3.63 ksi
ISO 37
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
300% Modulus 0.0250 GPa
3.63 ksi
ISO 37
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..