Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
ASTM D2240
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength 32.0 MPa
4640 psi
ASTM D412
Elongation at Break 480 %
480 %
ASTM D412
100% Modulus 0.0180 GPa
2.61 ksi
ASTM D412
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Tear Strength 180 kN/m
1030 pli
ASTM D624
Abrasion 60
60
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 195 - 210 °C
383 - 410 °F