Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00645 GPa | 0.936 ksi | Measured on solution cast film from toluene; BAM 1245 |
Kraton® A1536 H (SEBS) Linear Triblock Copolymer Description: Kraton A1536 H is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: Kraton A1536 HU - supplied to cu.. |