Mechanical Properties Metric English Comments
300% Modulus 0.0111 GPa
1.61 ksi
DIN 53504
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
300% Modulus 0.0111 GPa

@Temperature 145 °C,
Time 2100 sec
1.61 ksi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
LG Chemical SBR 1739 High Acrylonitrile Polymer
Description: SBR 1739 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 40% bound styrene. Raw materials for this p..
300% Modulus 0.0111 GPa

@Temperature 145 °C,
Time 2100 sec
1.61 ksi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
LG Chemical SBR 1789 High Acrylonitrile Polymer
Description: SSBR 1789 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (RAE type) oil and styrene-butadiene copolymer of 40% bound styrene. Raw materials for this product are ..
300% Modulus 0.0111 GPa
1.61 ksi
ASTM D412
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..