Mechanical Properties Metric English Comments
300% Modulus 0.0120 GPa
1.74 ksi
DIN 53504
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
300% Modulus 0.0120 GPa
1.74 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1118 B (SBS) Linear Triblock Copolymer
Description: Kraton D1118 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from South America in the physical form(s) identifi..
300% Modulus 0.0120 GPa
1.74 ksi
ISO 37
Kraton® D1118 E (SBS) Diblock Copolymer
Description: Kraton D1118 E is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from Europe in the physical form identified: D1118 ET - sup..
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude..
300% Modulus 0.0120 GPa
1.74 ksi
ISO 37
Huntsman AVALON® 90 AE Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.0120 GPa
1.74 ksi
ISO 37
Huntsman AVALON® 90 AHT DP Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.0120 - 0.0180 GPa
1.74 - 2.61 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1501 Styrene Butadiene Rubber
KRALEX® 1501 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin acids and contains 23.5% of chemically bonded ..
300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1712 Styrene Butadiene Rubber
KRALEX® 1712 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..
300% Modulus 0.0120 - 0.0180 GPa
1.74 - 2.61 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1721 Styrene Butadiene Rubber
KRALEX® 1721 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 40% ..
300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1723 Styrene Butadiene Rubber
KRALEX® 1723 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..
300% Modulus 0.0120 - 0.0180 GPa
1.74 - 2.61 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1732 Styrene Butadiene Rubber
KRALEX® 1732 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 32% ..
300% Modulus 0.0120 - 0.0180 GPa
1.74 - 2.61 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1739 Styrene Butadiene Rubber
KRALEX® 1739 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 40% ..
300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1778 Styrene Butadiene Rubber
KRALEX® 1778 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1490IV Polyester Based TPU
Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1685AD Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D638
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D638
ELASTO UK Dryflex® 422501S SBS Based Material, 50D Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.