Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0120 - 0.0170 GPa | 1.74 - 2.47 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1712 Styrene Butadiene Rubber KRALEX® 1712 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |
|||
300% Modulus | 0.0120 - 0.0170 GPa | 1.74 - 2.47 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1723 Styrene Butadiene Rubber KRALEX® 1723 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |
|||
300% Modulus | 0.0120 - 0.0170 GPa | 1.74 - 2.47 ksi | 35'/145°C; ASTM D412 |
SYNTHOS Kralex® 1778 Styrene Butadiene Rubber KRALEX® 1778 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5.. |