Polymer Property : 300% Modulus = 2.90 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go..
300% Modulus 0.0200 GPa
2.90 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1190 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0200 GPa
2.90 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 305ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
300% Modulus 0.0200 GPa
2.90 ksi
ISO 37
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.0200 GPa
2.90 ksi
ISO 37
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by..
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1295 Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0200 GPa
2.90 ksi
ISO 37
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..