Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength 30.0 MPa
4350 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
100% Modulus 0.0120 GPa
1.74 ksi
ASTM D412
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Tear Strength 120 kN/m
685 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Processing Properties Metric English Comments
Processing Temperature 195 - 215 °C
383 - 419 °F