Mechanical Properties Metric English Comments
300% Modulus 0.0229 GPa
3.32 ksi
ASTM D412
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection ..
300% Modulus 0.0229 GPa
3.32 ksi
ASTM D412
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b..