Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 93

@Time 5.00 sec
87 - 93

@Time 0.00139 hour
ASTM D2240
Tensile Strength 65.5 MPa
9500 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
300% Modulus 0.0229 GPa
3.32 ksi
ASTM D412
Flexural Modulus 0.0972 GPa
14.1 ksi
ASTM D790
Tear Strength 29.8 kN/m
170 pli
ASTM D470
Graves Tear Strength 105 kN/m
600 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4.5
4.5
H18, 1000g; ASTM D3389 B
Tensile Set 20 %
20 %
200% elongation; ASTM D412/D638
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
Kofler
175 °C
347 °F
DSC
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
DSC
Optical Properties Metric English Comments
Haze 23 %
23 %
pressed between glass; ASTM D1003
Processing Properties Metric English Comments
Zone 1 182 °C
360 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 193 °C
379 °F
Extrusion
Zone 4 199 °C
390 °F
Extrusion
Adapter Temperature 204 °C
399 °F
Extrusion
Die Temperature 204 °C
399 °F
Zone 1, Extrusion
204 °C
399 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume Swell in Water 1.8%
24h, 23°C; ASTM D471