Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0441 GPa | 6.40 ksi | |
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0441 GPa | 6.40 ksi | |
Taiwan Sheen Soon Sheenthane® D6010E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0441 GPa | 6.40 ksi | |
Taiwan Sheen Soon Sheenthane® D6320E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0441 GPa | 6.40 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S168D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0441 GPa | 6.40 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S375D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0441 GPa | 6.40 ksi | ASTM D412 |
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |