Mechanical Properties Metric English Comments
Impact Test 0.780 J
0.575 ft-lb
Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Impact Test 0.780 J
0.575 ft-lb
25 µm film; Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Impact Test 0.780 J
0.575 ft-lb
25 µm film; Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 500HN Polyimide Film, 125 Micron Thickness
Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).Genera..
Impact Test 0.780 J
0.575 ft-lb
25 µm film; Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 50HN Polyimide Film, 13 Micron Thickness
Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Impact Test 0.780 J
0.575 ft-lb
Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme..
Impact Test 0.780 J
0.575 ft-lb
25 µm film; Impact strength per DuPont Pneumatic Impact Test
DuPont™ Kapton® 200HN Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General ..