Polymer Property : Impact Test = 0.950 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 0.950 J
0.701 ft-lb
Dynatest, Penetration Energy; ISO 7765-2
Borealis Bormod™ HD905CF Polypropylene Homopolymer for Cast Film
Bormod HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recomme..
Impact Test 0.950 J
0.701 ft-lb
Dynatest, Penetration Energy; ISO 7765-2
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film
Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s..