Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Borealis
Trade Name Bormod™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is specifically designed to be coextruded as a stiff core layer with a copolymer coat layer of Borclear RE718CF. It is recommended to use rather high chill roll temperatures in the range of 40-55°C to obtain the optimum film stiffness. Optical properties will not be deteriorated as with conventional homopolymers at these temperatures.Bormod HD915CF is especially suitable for metallisable cast film (non migratory stabilizers/anti-acids), inner layer in coextrusion, twist films, labeling films, lamination films, furniture films, decorating films, and textile films.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.900 - 0.910 g/cc
0.0325 - 0.0329 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 80 %
80 %
ISO 527-3
Film Elongation at Break, TD 120 %
120 %
ISO 527-3
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Secant Modulus, MD 1.60 GPa
232 ksi
ISO 527-3
Secant Modulus, TD 1.80 GPa
261 ksi
ISO 527-3
Impact 40
40
Dynatest, Damaging Force (N); ISO 7765-2
Impact Test 0.950 J
0.701 ft-lb
Dynatest, Penetration Energy; ISO 7765-2
Coefficient of Friction 0.30 - 0.40
0.30 - 0.40
Film/Film; ISO 8295
Film Tensile Strength at Break, MD 35.0 - 55.0 MPa
5080 - 7980 psi
ISO 527-3
Film Tensile Strength at Break, TD 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 164 - 170 °C
327 - 338 °F
ISO 3146
Vicat Softening Point 158 °C
316 °F
A (10 N); ISO 306
Optical Properties Metric English Comments
Haze <= 6.0 %
<= 6.0 %
ASTM D1003
Gloss >= 90 %
>= 90 %
ASTM D2457
Users viewing this material also viewed the following: