Impact Test 105 J
77.4 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Impact Test 105 J
77.4 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Impact Test 105 J
77.4 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..