Mechanical Properties Metric English Comments
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC (Asia Pacific)
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC
LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI
LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region.
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO
LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su..
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp..
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific)
LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific)
LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0815A
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Impact Test 12.0 J
8.85 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific)
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE
LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific)
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp..
Impact Test 12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East)
LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.