Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 2.50 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 3.39 - 6.78 J
2.50 - 5.00 ft-lb
Torque Prevail
Ritelok TL42 Nutlock
Anaerobic. Medium strength threadlocker for screws, nuts and bolts. Prevent corrosion, Vibration resistant, Dismantle using normal tools
Impact Test 3.39 - 6.78 J
2.50 - 5.00 ft-lb
Prevail
ND Industries NutGrade® 121 Removable Threadlocker
A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th..
Copyright © lookpolymers.com All Rights Reserved