ND Industries NutGrade® 121 Removable Threadlocker

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name NutGrade®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries NutGrade® 121 Removable Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger than .25" in diameter.Meets military spec MIL-S-46163 Type II Grade N
Physical Properties Metric English Comments
Viscosity 1200 - 1500 cP
1200 - 1500 cP
Thixotropic
Mechanical Properties Metric English Comments
Impact Test 3.39 - 6.78 J
2.50 - 5.00 ft-lb
Prevail
11.3 - 22.6 J
8.33 - 16.7 ft-lb
Break
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
With Primer (Fixture)
20.0 min
0.333 hour
On steel (fixture)
1440 min
24.0 hour
With Primer (Full)
1440 min
24.0 hour
On steel (Full)
Descriptive Properties Value Comments
Color Blue
Gap Fill, in. 0.005