Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 6.10 J | 4.50 ft-lb | Falling weight impact per ASTM D3029 GB |
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio.. |
|||
Impact Test | 6.10 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Impact Test | 6.10 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Impact Test | 6.10 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Impact Test | 6.10 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Impact Test | 6.10 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Impact Test | 6.10 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.50 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ARM impact |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Impact Test | 6.10 J | 4.50 ft-lb | |
Parkway Products Thixomolded® AM60A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |