Impact Test 6.10 J
4.50 ft-lb
Falling weight impact per ASTM D3029 GB
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio..
Impact Test 6.10 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD8020 Polypropylene
DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 6.10 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD8020 Polypropylene
DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 6.10 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD8020 Polypropylene
DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 6.10 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD8020 Polypropylene
DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 6.10 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD8020 Polypropylene
DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 6.10 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.50 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
A. Schulman POLYAXIS® PD8020 Polypropylene
DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 6.10 J
4.50 ft-lb
Parkway Products Thixomolded® AM60A Magnesium
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate..