Polymer Property : Impact Test = 50.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 67.8 J

@Temperature -40.0 °C
50.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM STD test
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel..
Impact Test 67.8 J

@Temperature -40.0 °C
50.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM STD test
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds.High quality Polyethylene re..
Impact Test 67.8 J

@Temperature 23.0 °C
50.0 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer  (discontinued **)
ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle..
Impact Test 67.8 J

@Temperature 23.0 °C
50.0 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer  (discontinued **)
ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he..
Impact Test 67.8 J
50.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Impact Test 67.8 J
50.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..