Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 67.8 J @Temperature -40.0 °C |
50.0 ft-lb @Temperature -40.0 °F |
0.125 in.; ARM STD test |
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel.. |
|||
Impact Test | 67.8 J @Temperature -40.0 °C |
50.0 ft-lb @Temperature -40.0 °F |
0.125 in.; ARM STD test |
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds.High quality Polyethylene re.. |
|||
Impact Test | 67.8 J @Temperature 23.0 °C |
50.0 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
Impact Test | 67.8 J @Temperature 23.0 °C |
50.0 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
Impact Test | 67.8 J | 50.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Impact Test | 67.8 J | 50.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |