Mechanical Properties Metric English Comments
Impact Test 82.7 J

@Thickness 3.17 mm,
Temperature -40.0 °C
61.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Impact Test 82.7 J

@Thickness 3.17 mm,
Temperature -40.0 °C
61.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Impact Test 82.7 J

@Thickness 3.17 mm,
Temperature -40.0 °C
61.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Impact Test 82.7 J

@Thickness 3.17 mm,
Temperature -40.0 °C
61.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Impact Test 82.7 J

@Thickness 3.17 mm,
Temperature -40.0 °C
61.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..
Impact Test 82.7 J

@Thickness 3.17 mm,
Temperature -40.0 °C
61.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle..