Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 82.7 J @Thickness 3.17 mm, Temperature -40.0 °C |
61.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Impact Test | 82.7 J @Thickness 3.17 mm, Temperature -40.0 °C |
61.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Impact Test | 82.7 J @Thickness 3.17 mm, Temperature -40.0 °C |
61.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Impact Test | 82.7 J @Thickness 3.17 mm, Temperature -40.0 °C |
61.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Impact Test | 82.7 J @Thickness 3.17 mm, Temperature -40.0 °C |
61.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Impact Test | 82.7 J @Thickness 3.17 mm, Temperature -40.0 °C |
61.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |