Mechanical Properties Metric English Comments
Heat Seal Strength 250 g/25 mm

@Time 0.250 sec,
Pressure 0.0345 MPa
0.551 lb/in

@Time 0.0000694 hour,
Pressure 5.00 psi
120°C, 35% RH
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin..