Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nominal 50 and 100 gauges. The film is typically provided with the sealant side wound toward the core. General Product Info: This film is similar to Mylar® OL2, however, this film will have much stronger seals at temperatures above 180°F than OL2. This film withstands freezing temperatures down to -40°F. Mylar® CL softens in the range of 425°-450°F.Typical Applications: This film when laminated to foil makes an excellent inner cap seal for PET jars. This film is also suitable for heating food products in microwave or conventional ovens.Approvals: FDA Food Contact Status - All gauges of Mylar® CL comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® CL can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Water Vapor Transmission 20.2 g/m²/day
1.30 g/100 in²/day
E96 Procedure E
Coating Weight 34.9 g/m²
21.8 lb/ream
0.5 m<sup>2</sup>; E252
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 140 %
140 %
ASTM D882
Film Elongation at Break, TD 80 %
80 %
ASTM D882
Tensile Modulus 3.79 GPa
550 ksi
ASTM D822
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
Film Tensile Strength at Break, MD 186 MPa
27000 psi
ASTM D882
Film Tensile Strength at Break, TD 276 MPa
40000 psi
ASTM D882
Heat Seal Strength 250 g/25 mm

@Time 0.250 sec,
Pressure 0.0345 MPa
0.551 lb/in

@Time 0.0000694 hour,
Pressure 5.00 psi
120°C, 35% RH
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Maximum Service Temperature, Inert -40.0 °C
-40.0 °F
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Descriptive Properties Value Comments
Gas Permeability (Base film) 5 cc/100 in2
O2, 24 hr; ASTM D3985 (77°F/75% RH/1 ATM)
Yield (nominal) 19900 in2/lb
Users viewing this material also viewed the following: