Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87707 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87717 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12 Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided .. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by.. |
|||
Izod Impact, Notched | 0.160 J/cm @Temperature -20.0 °C |
0.300 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem Prisma 2400 RACO Random Polypropylene Copolymer Prisma 2400 is a high melt flow rate random copolymer. This product is designed for the ISBM (Injection Stretch Blow Molding) process and offers low taste/odor. It can also be used in the blow moldi.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9175 White 10 Rigid PVC, Molding, White 10 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |