Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.267 J/cm @Temperature -20.0 °C |
0.500 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Dow 6D20 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature -20.0 °C |
0.500 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Dow R131-02A Polypropylene Random Copolymer Resin DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature -20.0 °C |
0.500 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Dow R132-02A Polypropylene Random Copolymer Resin DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12 Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided .. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 6.35 mm, Temperature -20.0 °C |
0.500 ft-lb/in @Thickness 0.250 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall CL-7053 Rigid PVC, Molding Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9175 White 10 Rigid PVC, Molding, White 10 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
0.500 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9301 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li.. |