Polymer Property : Izod Impact, Notched = 0.500 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.267 J/cm

@Temperature -20.0 °C
0.500 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Dow 6D20 Polypropylene Random Copolymer Resin
OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr..
Izod Impact, Notched 0.267 J/cm

@Temperature -20.0 °C
0.500 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Dow R131-02A Polypropylene Random Copolymer Resin
DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Izod Impact, Notched 0.267 J/cm

@Temperature -20.0 °C
0.500 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Dow R132-02A Polypropylene Random Copolymer Resin
DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12
Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided ..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38
Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by..
Izod Impact, Notched 0.267 J/cm

@Thickness 6.35 mm,
Temperature -20.0 °C
0.500 ft-lb/in

@Thickness 0.250 in,
Temperature -4.00 °F
ASTM D-256
Axiall CL-7053 Rigid PVC, Molding
Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9175 White 10 Rigid PVC, Molding, White 10
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38
Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.500 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..