Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.333 J/cm @Thickness 6.35 mm |
0.625 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.333 J/cm @Thickness 6.35 mm |
0.625 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR Information provided by Samsung Cheil Industries. |