Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.180 J/cm @Temperature 23.0 °C |
0.337 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP563 ABS SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.180 J/cm @Temperature -20.0 °C |
0.337 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem Symbios 3102 Polypropylene Terpolymer Braskem Symbios 3102 is a medium melt flow rate terpolymer with a heat seal temperature below 110ºC on its non-treated face. It is designed for use as a heat sealing layer for cast film coextrusion.. |
|||
Izod Impact, Notched | 0.180 J/cm @Temperature -20.0 °C |
0.337 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem RP 145 RACO Random Polypropylene Copolymer RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellen.. |