Polymer Property : Izod Impact, Notched = 0.481 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.481 J/cm

@Temperature -20.0 °C
0.900 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
Ineos L34N-00 Polypropylene Impact Copolymer
Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in..
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
0.900 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8015 CL
Availability: North AmericaForms: PelletsFeatures: CopolymerAppearance: Clear/TransparentInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.900 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS LE WT
Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.